|Japanese Foreign Ministry to help its Startups, Small and Medium industry to enter India | The Japan-India Economic Affairs Division will encourage Japanese companies to expand investment and presence in India | The Ministry has urged India to remove or reduces regulatory challenges | Jiji Press reports there were about 1400 Japanese companies in India in 2024, the same as in 2018 | Gurgaon-based Maruti Suzuki, owned by Suzuki, is among the top Japanese companies in India | Indian Defence Ministry working on Deeper Civil-Military Technology Cooperation | India attracts $40 billion in FCNR (B), or Foreign Currency Non Resident (Bank) deposits, in two months from overseas Indians | A similar scheme, with better interest rates in 2013, had attracted $26 billion | Ngulkham Jathom Gangte, IFS Batch 1994, is appointed as India’s Ambassador to Mexico | He is currently serving as Special Secretary in the Ministry of External Affairs | Congratulations, Ambassador. 🎉💫 | Trump Threatens to Bomb Bridges and Power Plants In Iran Every Time it Attacks Ships in Strait of Hormuz | Captain Shivani Sehrawat creates history by becoming the First Woman ADC to the Indian Army’s Chief of Staff | Maldova Presudent Maia Sandu says her country can be Gateway to Europe for Indian businesses | India and China will gave differences but they Should Not Become Disputes, says Jaishankar | Trump Approves 30-year Civil Nuclear Cooperation Agreement with Saudi Arabia | India Strategic Greets President Emmanuel Macron and the People of France on their National Day 14 of July | Viva la France | Qatar mourns passing away of former Emir Shaikh Hamad bin Khalifa Al Thani. He was 74 | Australia to supply Uranium to power Indian Reactors after Modi, Albanese announce agreements on Defence and Nuclear Energy | Modi, New Zealand PM Christopher Luxon elevate ties to Strategic Partnership | 12 Pacts include cooperation in Indo-Pacific and Logistics Support to Naval Ships | Bilateral trade to double to about US $ 4 billion by 2030 | Indian Navy Commissions 6th Nilgiri class Stealth Frigate INS Mahendragiri | Future Wars will use AI but will be won by Trained Soldiers and Robust Military Power, says Rajnath Singh | Akashvani, the popular state-run All India Radio, is 90 | China recovers Reusable Rocket, as visualised in the 1962 James Bond film Dr No | US Elon Musk’s SpaceX was the First to do so, and China follows as the Second | Modi in Indonesia, and then Australia and New Zealand to strengthen Indo-Pacific partnerships | Defence, Minerals, AI top agenda | Jaishankar commends Qatar’s role in Iran-US Peace Talks | India building Semiconductors and Electronics clusters, in collaboration with Japanese and other companies: PM Modi | China conducts rare Submarine Launched Ballistic Missile Test, the first since 1980 | India Joins UN Global Dialogue on Artificial Intelligence in Geneva July 6-7 | LNG supplies resume through Strait of Hormuz after US, Iran Ceasefire | 15 of 20 Indian Fertiliser ships stuck in Hormuz set sail | India sourced Fuel from 40 countries during the Hormuz closure, says Modi | Modi signing Agreements with Australia to buy Uranium and Minerals | India creates 900 million Unique Health IDs towards Digital health ecosystem | India to double Gas buys from US from existing 2.2 million tonnes of LPG | Trump says Iran’s Nuclear Programme Obliterated in US bombings | Egypt inaugurates its new 22-acre Defence HQ, shaped as Octagon | US Celebrates 250 Years of Democracy, History and Power | India Strategic Greets All American Friends on this Blessed Occassion🙏😇🎉♥️💫 | India, Japan to boost bilateral trade from the existing $25b | Japan interested in utilising ISRO rockets for Space launches | Shipbuilding major for Japan or frigates Air Land and Naval Specific issues will cone on the table | J projects look at Notth East Think Tank exchanges | Semiconductor being developed in Assam with Japan Enhancing bilateral cooperation | Imp of quad Of co-op in info pacific | General Dhiraj Seth Took Over as India’s 31st Army chief on June 30 | He succeeds Gen Upendra Dwivedi who Retired after 40 Years of service | Gen Seth was commissioned into the Armoured Corps in 1986 | Gen Seth has commanded Strike formations and was also GOC of the important Delhi Area | India to Warmly Welcome Japanese PM Sanae Takaichi July 1-3 for Annual Summit | India sends Portable Field Hospital to Venezuela along with Doctors and Medicines | 41 Indian Army Para Field personnel sent under Op Amistad, or Friendship | Two IAF Boeing C 17 fly 15,000 km with Medics and Equipment to the faraway Friends | Iran reiterates exclusive right to control Strait of Hormuz | Iran also warned Safe Passage cannot be assured for Ships sailing away from its designated channels | Six Arab Gulf States call for Restoration of Freedom of Navigation in the strategic Strait | Iran warns: “Gulf States’ strategic survival at Mercy of Tehran’s Tolerance” | India, Switzerland to deepen Science and Tech Ties | Starmer resigns as UK Prime Minister amid mounting Labour Party pressure | US, Iran War Ends with a Binding Commitment from Iran to Never Produce Nuclear Weapons | Oil Starts Flowing Freely Through Strait of Hormuz | US and Iran both Allow Movement of Oil Tanker’s | ONGC to Invest $1.5 billion to Boost India’s Oil Storage by 33 % | Qatar Amir-gifted Boeing 747 is new US Air Force Presidential Jet | Meta and Reliance to set up a huge Global Digital Hub in Jamnagar | Modi, Trump meet warmly again, this time at G7 | Modi showers praise on Trump for his Middle East peace effort | Trump says We always had Tremendous Relationship with India | Trump praises Modi, jovially calling him ‘a killer’ for his negotiating skills at G7 | Modi said Freedom of Navigation in the Strait of Hormuz is A Must | Trump expressed condolences for the Indian sailors killed in US Navy attack in the Gulf | Trump said US and Iran will sign an MoU to end their war on Friday June 19 | All the G7 Leaders supported the Peace Effort | Modi, UAE President Shaikh Mohammed agree to work together on Middle East Peace, Security and Stability | Piyush Goyal discusses expanding partnership with Prince Albert II of Monaco
DEFENCE INDUSTRYTECHNOLOGY

Rajnath Singh dedicates titanium and superalloy plant in Lucknow, calls for India to produce rare defence materials

New Delhi, October 18. Defence Minister Rajnath Singh on October 18 dedicated to the nation a Titanium and Superalloy Materials Plant at PTC Industries’ Strategic Materials Technology Complex in Lucknow, urging that India must produce rare and critical materials used in defence and aerospace to safeguard its technological sovereignty and emerge as a technology creator.

Defence Minister Rajnath Singh addressing at the inauguration of the Titanium & Superalloy Materials Plant at PTC Industries’ Strategic Materials Technology Complex, in Lucknow, Uttar Pradesh on October 18, 2025.

Emphasising the strategic importance of rare earth materials used in defence, space, and electronics, Singh said that only a few nations currently possess the capability to refine and process such materials. He noted that the new facility – among the first private-sector plants in India to manufacture aero-engine and superalloy components – would play a crucial role in reducing dependence on imports and enabling indigenous production of advanced materials.

‘True strength lies in manufacturing our own materials’

Reflecting on India’s earlier reliance on foreign countries for advanced materials, Singh said the new plant marks a turning point in the country’s quest for self-reliance.

“India will achieve real strength only when it can make its own materials, components, chips, and alloys,” he said. “With this facility, India joins an elite group of nations capable of producing critical materials for fighter jets, missiles, naval systems, and satellites.”

The Defence Minister stressed that while technology is power, “material is the real strength”, as no high-end system – from semiconductors to turbine engines – can exist without it. He described the plant as a foundation for India’s technological sovereignty and a “living example of Aatmanirbhar (self-reliant) Bharat,” with benefits extending from industry to society.

Defence Minister Rajnath Singh inaugurates Titanium & Superalloy Materials Plant at PTC Industries’ Strategic Materials Technology Complex, in Lucknow.

Boost to UP’s industrial ecosystem

Praising the project’s contribution to Uttar Pradesh’s industrial landscape, Singh said the Strategic Materials Technology Complex would create direct and indirect employment opportunities and attract supplier industries and startups to the region.

“The UP Defence Industrial Corridor is on its way to becoming one of Asia’s most advanced manufacturing zones,” he said, adding that it would provide technical training and employment to youth across the state.

Singh commended Chief Minister Yogi Adityanath for Uttar Pradesh’s transformation over the past decade, citing improved law and order, investor confidence, and the rise of factories, IT hubs, and research centres that have made the state a “growth engine of the nation”.

Mr. Rajnath Singh at the Titanium & Superalloy Materials Plant at PTC Industries’ Strategic Materials Technology Complex in Lucknow on October 18, 2025.

India moving from ‘Make in India’ to ‘Design, Develop and Deliver in India’

Highlighting the growing role of the private sector in defence manufacturing, the Defence Minister said India has moved beyond ‘Make in India’ to a new phase of ‘Design, Develop and Deliver in India’. He urged startups, MSMEs, and innovators to view participation in the defence sector as not just a business opportunity but a national responsibility, assuring full government support and policy backing.

Major collaborations and achievements

During the event, a memorandum of understanding (MoU) was signed between PTC Industries and Bharat Dynamics Limited (BDL) to jointly develop propulsion systems, guided bombs, and small aero-engines for missiles, UAVs, and loitering munitions – a move expected to accelerate the indigenisation of advanced propulsion technologies.

PTC Industries also received multiple Letters of Technical Acceptance (LoTAs) from the Centre for Military Airworthiness and Certification (CEMILAC) under DRDO for:

  • Titanium Rear Fin Root Castings for the Advanced Medium Combat Aircraft (AMCA), developed in collaboration with DMRL and ADA.
  • Oil Tank Assembly Titanium Castings for the Kaveri Derivative Engine (KDE-2), in partnership with GTRE.
  • A Purchase Order for post-cast operations to manufacture single-crystal turbine blades for the KDE-2 – a significant milestone in developing one of the most complex components in modern jet engines.

Spread over 50 acres and established with an investment of Rs. 1,000 crore, the complex has a production capacity of over 6,000 tonnes per annum, enabling India to produce aviation-grade titanium and superalloys from domestic and recycled sources – a decisive move towards strategic materials independence.

Singh, accompanied by Chief Minister Yogi Adityanath, Deputy Chief Minister Brajesh Pathak, DRDO Chairman Samir V Kamat, and BrahMos DG Jaytirth R Joshi, also toured the facility and reviewed its advanced manufacturing infrastructure.